  • Inconel X 750 The Aging Strengthening Nickel Based Superalloy - China

    price: contact company for price

    InconelX-750(NO7750) the aging strengthening nickel-based superalloy

    Features and applications overview: InconelX-750 is a nickel-base

    superalloy aging strengthened by γ'[Ni3(Al, Ti, Nb)]

    phase, and has good corrosion resistance and oxidation resistance under

    980°C, rather high strength under 800°C, quite good resistance under

    540°C. It also has good formability and weldability. The alloy is mainly

    for manufacturing high-strength and corrosion resistant annulus parts,

    structural parts, bolts, and other parts of aircraft engine operating at

    800°C, and flat springs and coil springs with medium or lower stress and

    relaxation resistance working at 540°C. It can also be used for

    manufacturing turbine blades of gas turbine and other parts. InconelX-

    750's similar grades: GH4145

    GH145(China), NCl5FeTNbA(France), W.Nr.2.4668

    NiCr15Fe7TiAl(Germany) NCF750(Japan) Chemical composition, %: Nickel +

    Cobalt...........................70 min Chromium..................................14.0-

    17.0 Iron.............................................5.0-9.0

    Carbon........................................0.08 max

    Manganese..................................1.0 max

    Silicon.........................................0.05 max

    Sulfur...........................................0.01 max

    Copper..........................................0.5 max Aluminium....................................0.4-

    1.0 Titanium........................................2.35-2.75 Physical

    properties Density, g/cm3 ..........................8.25 Melting

    Range, °C.....................1395-1425 Thermal conductivity,

    λ/(W/m•°C), at 100°C .............14.7 Specific heat,

    J/kg•°C..............430 Elastic modulus, GPa..............214

    Electrical resistivity, μΩ•m......1.22 Coefficient of linear

    expansion,

    a/10-6°C-1, at 20-100°C.............13.1

    Mechanical properties (the minimum value detected at room temperature)

    Tensile strength, σb/MPa..............930

    Yield strength, σp0.2/MPa.........515

    Elongation, σ5 /%.............................30

    The way of heat treatment is solution treatment

    Available products and specifications:

    Bar: ASTM B637, AMS 5667, AMS 5668, AMS 5669, AMS 5670, AMS 5671, AMS 5741, AMS 5749, ASME SB637

    Forging: ASTM B637, AMS 5667, AMS 5668, AMS 5670, AMS 5671, AMS 5747, AMS 5749, ASME SB637

    Plate/Strip: AMS 5542, AMS 5598

    Wire: AMS 5698, AMS 5598

    Pipe: AMS 5582

    The metallurgical structure of Inconel X-750:

    The structure of the alloy in the state of standard heat-treatment consists of γ matrix, Ti(C, N), Nb(C, N), M23C6 carbides and γ'[Ni3(Al, Ti, Nb)] phase. γ' is the main strengthening phase of the alloy and it accounts for 14.5%.

    The process performance and requirements of Inconel X-750:

    The alloy is easy to shape when the forging temperature is between 950 and 1220°C. The solution treatment follows the intense molding step.

    The average size of the grain size of the alloy is closely related to the forging deformation degree and the final forging temperature.

    The alloy has good weldability and is suitable for any welding. Aging treatment after welding enables the alloy to obtain the strength of near perfect heat treatment.

    The heat processing of the parts shall be operated in the sulfur-free neutral or reducing atmosphere in order to avoid vulcanization.

    Inconel X 750 The Aging Strengthening Nickel Based Superalloy

    Please see our contact information below


    Company Contact:


    • Phone: 8602169925078

    • Address: 1355#,Chengbei road, Jiading District, Shanghai, Shanghai, China

    • Email: Email


    Published date: October 19, 2012 -

    • Business Description: involved in international trade import export of goods, products, and services

    Related listings



    • Nimonic 90 Aging Hardening Nickel Based Wrought Superalloy
      Nimonic 90 Aging Hardening Nickel Based Wrought Superalloy
      General Metals - Shanghai Kangsheng Superalloy Co., Ltd - China - October 19, 2012 - contact company for price

      Nimonic90 aging hardening nickel-based wrought superalloy Features and applications overview: Nimonic90 is age hardenable nickel-based wrought superalloy containig a higher amount of cobalt and a variety of strengthening elements. The alloy has rathe...

    • Nimonic 93 Precipitation Hardening Nickel Based Alloy
      Nimonic 93 Precipitation Hardening Nickel Based Alloy
      General Metals - Shanghai Kangsheng Superalloy Co., Ltd - China - October 19, 2012 - contact company for price

      Nimonic93 precipitation hardening nickel-based alloy Nimonic93's features and applications overview: This alloy is a precipitation hardened nickel based alloy containing higher amount of cobalt and chromium. It has high strength and good microstructu...

    • Elegant And Unique Metal Vertical Blind
      Elegant And Unique Metal Vertical Blind
      General Metals - Anguo city sorter world netting - China - October 13, 2012 - contact company for price

      Metal vertical blinds our products were designed by the world famous designers and at the same time with high quality, droopily drapery , natural transparency , you can use it to easily create a romantic atmosphere, with Good decorative role. I belie...



    Safe Trade Tips

    • Ask for business references and check them
    • Use a payment method that offers better protection for all such as Letters of credit and verified professional escrow services. Avoid payments in advance such as money transfers
    • Verify their business via their local Chamber of Commerce
    • Search the internet using their website address, their business name, their phone and fax numbers, and their email addresses to see if you can find any feedback about them.
    • Get to know more about scams to avoid: Internet Crime Complaint Center - International Financial Scams
    • This site is never involved in any transaction, and does not handle payments, shipping, guarantee transactions, provide escrow services, or offer "buyer protection" or "seller certification"